I'm curious to know if the QR tweeter foil delaminates less than, not at all, or about the same as the wire mid base panels of 1.6s and lower. In my mind at least, it would make sense that the foil adheres better with the increased and flat surface area. If the foil tends to delaminates less or not at all, for me it makes a point in favor of upgrading to 1.7s or .7s when they become available, since they are entirely QR.
LineSource
Edits: 09/12/14
This post is made possible by the generous support of people like you and our sponsors:
Topic - Does QR Tweeter Foil Delaminate Less? - LineSource 13:01:04 09/12/14 (1)
- RE: Does QR Tweeter Foil Delaminate Less? - JBen 20:20:51 09/12/14 (0)